Answers · from Chapter 39: Insulators & Dielectrics

Does insulation life halve for every 10 °C rise?

Does insulation life halve for every 10 °C rise?

The rule that insulation life halves with each 10 °C rise holds only roughly, as a rule of thumb. Organic insulation ages through chemistry, and the reaction runs faster when hot, and manuals print a halving step of 8 to 10 °C. The step depends on the material, among other limits, and Chapter 39 rates the rule Plausible.

Evidence rating: Plausible. Claim rated: "Insulation life halves for every 8-10 °C rise in temperature". How the ratings work.

Where the rule comes from

In 1930 V. M. Montsinger, studying oil-paper transformer insulation, reported that its aging rate roughly doubled with each 8 °C rise. T. W. Dakin supplied the explanation in 1948: he showed that aging is a chemical reaction whose rate follows the Arrhenius law. Plot the logarithm of insulation life against the reciprocal of absolute temperature and the points fall on a straight line. A fixed temperature step then multiplies life by a fixed factor over the range where that line holds.

Chapter 39 notes that both papers are known to the author only through a 2011 CERN review by D. Tommasini, and that Montsinger's own figure is reported as 8 °C even though the rule bearing his name is usually quoted as 10 °C.

How the manuals state it

Official manuals disagree on the size of the step. The Bureau of Reclamation's transformer maintenance manual of 2000 says that running only 10 °C above rating cuts transformer life by half. A 2005 Reclamation document gives both 8 °C and a range of 8 to 10 °C. The Department of Energy's 2014 motor guide calls the 10 °C figure an often stated rule of thumb.

The same Arrhenius basis underlies insulation thermal classes. For US motors, with 40 °C surroundings and a 1.0 service factor, the DOE gives limits near 100 °C for Class A, 120 °C for B, 145 °C for F and 165 °C for H. A class covers the complete insulation system, including wire, varnish and slot liner, rather than any single material.

Why the chapter stops at Plausible

The book's evidence box rates the claim Plausible. The halving step changes with the material and with which reaction is doing the damage. The rule holds only while a single aging reaction dominates. It ignores moisture, oxygen, vibration and electrical stress; Reclamation's manual adds that each doubling of moisture in a transformer halves its insulation life. And no rule of this kind can give the remaining life of any one machine.

What would settle it for a given insulation system is an Arrhenius endurance test under IEC 60216-1, which measures the halving step directly. No single universal number has been shown.

What Chapter 39 covers

Chapter 39 covers the Leyden jar and Faraday's permittivity measurements, dielectric strength and loss, puncture, tracking and partial discharge, the classic insulating materials, PCBs and silicone fluids, and thermal aging.

Sources

  • D. Tommasini, Dielectric insulation and high-voltage issues, CERN Accelerator School, arXiv:1104.0802 (2011)
  • V. M. Montsinger, Loading transformers by temperature, AIEE Transactions 49 (1930)
  • T. W. Dakin, AIEE Transactions 67 (1948)
  • US Bureau of Reclamation, FIST 3-30, Transformer Maintenance (2000)
  • US Bureau of Reclamation, Transformers: Basics, Maintenance, and Diagnostics (2005)
  • US DOE, Premium Efficiency Motor Selection and Application Guide (2014)

Read more in Chapter 39: Insulators & Dielectrics, part of Volume II: System Anatomies. All answers · Formats and prices