Volume II · Part IX: Materials: How the Parts Come to Exist · Chapter 40
Cells & Batteries
Planté's lead cell, the dry cell, sulfation, Edison's nickel-iron battery and LFP versus NMC lithium cells, with measured figures.
A guide to the chapter, written for this site. It describes the chapter; it is not an extract from it.
What the chapter covers
This chapter describes how cells make and store current, from the first batteries to the two lithium chemistries that now lead stationary storage. It opens in March 1860 with Gaston Planté showing the Paris Academy a battery of nine lead cells that gave back what it had been charged with. It then steps back to Volta's pile of 1800, Daniell's two-liquid cell, the Weston cadmium standard, and the Leclanché and Gassner cells that led to the dry cell of 1888. The lead-acid section explains the double-sulfate reaction, why a hydrometer reads state of charge, the Bureau of Standards' 1920 voltages and charging limits, Planté's slow formation of plates and the Faure pasted grid. A section on sulfation lists the four abuses the Bureau named and what care amounts to. Edison's nickel-iron cell of 1901 is read against the words of his own patent and the later measurements: an unchanged electrolyte, about 70 percent charge efficiency measured for commercial iron electrodes and energy per kilogram near lead-acid. The lithium section compares LFP and NMC cells on energy, cycle life, round-trip efficiency and a 2025 thermal-runaway test. A safety box covers hydrogen, acid and caustic, lead, short circuits and lithium fire, each with the federal or international source the chapter cites.
Claims the chapter rates
Each claim gets one rating on the book's scale. How the ratings work.
| Claim | Rating | Kind |
|---|---|---|
| Nickel-iron batteries last for decades (popular claim: they last forever) | Plausible | empirical |
| LFP cells are safer in thermal runaway than NMC cells | Plausible | empirical |
Key numbers
- Nickel-iron cell, open circuit / working average
- 1.45-1.52 V / about 1.14 V (NBS Circular 92 (1920))
- Lead-acid specific gravity, charged / discharged
- 1.275-1.290 / 1.115-1.130 (NBS Circular 92 (1920))
- LFP / NMC / lead-acid cycle life (80 % DOD, end at 80 % energy)
- 2,400 / 1,520 / 1,370 (PNNL-33283 (2022))
- Charge efficiency of commercial iron electrodes
- about 70 % (Narayan et al. (2015))
- Hydrogen flammable range in air
- 4-75 % by volume (ILO/WHO ICSC 0001 (2014))
Questions this chapter answers
How long does a nickel-iron (Edison) battery last?
The chapter rates Plausible the claim that nickel-iron batteries last for decades. The plates are not used up and the electrolyte keeps its composition, and a 2023 review gives service lives as long as 25 years. No published capacity record over many decades was found, and "forever" rests on anecdote. For battery installations, check the code in force where you are.
What causes sulfation in a lead-acid battery?
Fine lead sulfate formed on discharge coarsens if the battery stands discharged, filling the plate pores and slowing the next charge. The Bureau of Standards in 1920 blamed four abuses, among them standing discharged and regular undercharging, and PNNL in 2022 tied faster decline to long storage at low charge. For battery installations, check the code in force where you are.
Are LFP lithium batteries safer than NMC batteries?
The chapter rates Plausible the claim that LFP cells are safer than NMC in thermal runaway. A 2025 test compared them directly: LFP released 0.02 mol gas per ampere-hour, NMC 0.07, and the LFP gas peaked at 446 °C, NMC's at up to 1,050 °C. LFP's gas was 41 percent hydrogen, and one cell of each type was tested. For battery installations, check the code in force where you are.
Why does a charging battery need ventilation?
Flooded cells give off hydrogen while charging, and hydrogen is flammable at 4 to 75 percent by volume in air (ILO/WHO ICSC 0001). The chapter cites 29 CFR 1926.441, the US construction rule that puts unsealed batteries in vented enclosures or well-ventilated rooms. For battery installations, check the code in force where you are.
Selected sources
- G. Planté, The Storage of Electrical Energy, trans. P. B. Elwell (1887)
- T. A. Edison, US Patent 678,722, Reversible Galvanic Battery (1901)
- US Bureau of Standards, Operation and Care of Vehicle-Type Batteries, NBS Circular 92 (1920)
- US Bureau of Standards, Electrical Characteristics and Testing of Dry Cells, Circular 79 (1919)
- V. Viswanathan, K. Mongird et al., 2022 Grid Energy Storage Technology Cost and Performance Assessment, PNNL-33283 (2022)
- S. R. Narayan et al., High Efficiency Nickel-Iron Battery, US 2015/0086884 A1 (Narayan et al. 2015)
- J. M. E. Abarro et al., Batteries 9 (2023), 383
- J. P. Barton, R. J. L. Gammon, A. Rahil, Frontiers in Energy Research 8 (2020), 509052
- G. Ferdigg and C. Mair, NVPF Sodium-Ion Versus NMC and LFP Lithium-Ion Batteries in Thermal Runaway, Batteries 11 (2025), 323
- ILO/WHO, International Chemical Safety Card ICSC 0001, Hydrogen (2014)
- 29 CFR 1926.441(a)(1)-(6), US construction rules for batteries
- NFPA 855, Standard for the Installation of Stationary Energy Storage Systems
- How long does a nickel-iron (Edison) battery last?
- Glossary: Nickel-iron cell
- Glossary: Planté cell
Related chapters
This chapter is in Volume II: System Anatomies. Drafted and twice audited; chapter text final. Formats and prices · All chapters