Volume II · Part IX: Materials: How the Parts Come to Exist · Chapter 41
Rectifiers & Detectors
Braun's 1874 crystal contact, the catwhisker, copper-oxide and selenium plates, the aluminum valve, Fleming's diode and the p-n junction.
A guide to the chapter, written for this site. It describes the chapter; it is not an extract from it.
What the chapter covers
This chapter follows the one-way valve for electric current from a lump of mineral to the transistor. It opens in Leipzig in November 1874, where Ferdinand Braun found that the resistance of metal sulfide contacts changed with the direction of current by up to 30 percent. It explains why batteries, plating and radio reception all need current that flows one way, and what makes a rectifier good. Radio gave Braun's contact a use: Bose's galena detector of 1904, Pickard's silicon detector of 1906 and the catwhisker crystal set, which needs no battery. A rated box takes up the early idea that these detectors worked by heating, and a plain section explains the barrier layer that does the work. Grondahl's copper-oxide plates and the selenium plates developed alongside them brought the same physics to battery chargers and instruments around 1930. The Bureau of Standards' 1924 tests of aluminum electrolytic valves give efficiencies for several charger types. Fleming's 1905 vacuum diode and De Forest's grid follow, then Ohl's p-n junction and the Bardeen-Brattain and Shockley transistor patents. A second rated box asks what a failing selenium rectifier gives off, and a safety box gives the NIOSH limits for selenium and hydrogen selenide and the hazards of old tube equipment.
Claims the chapter rates
Each claim gets one rating on the book's scale. How the ratings work.
| Claim | Rating | Kind |
|---|---|---|
| Crystal detectors rectify at a contact barrier, not by heating the contact | Proven | empirical |
| A failing selenium rectifier gives off hydrogen selenide | Untested | empirical |
Key numbers
- Braun's direction-dependent resistance, metal sulfides
- up to 30 % (Braun (1874))
- Pickard silicon detector, claimed efficiency
- "upward of ten per cent" (patent claim) (US 836,531 (1906))
- Copper-oxide plate, reverse/forward resistance ratio as clamping rose
- about 27.5 to about 120 (US 1,640,335 (1927))
- Aluminum rectifier charging 24 lead cells, efficiency
- 55-59 % (transformer loss excluded) (NBS Technologic Paper 265 (1924))
- Barrier-layer depth (1939 theory)
- about 10^-4 cm (Pearson and Brattain (1955))
Questions this chapter answers
How does a crystal radio detector work?
A fine wire, the catwhisker, touches a crystal such as galena or silicon, and the contact passes current more readily one way. That cuts away one half of the radio carrier, leaving an average that follows the speech or Morse signal. The antenna powers the earphone, so the set needs no battery.
How do copper-oxide and selenium rectifiers work?
Copper-oxide and selenium rectifiers are each a large-area junction between a metal and a semiconductor layer, with a thin barrier that passes current easily one way. Grondahl's 1927 patent formed the oxide on copper; selenium was coated onto a metal plate and topped with a sprayed alloy contact. Plates were usually stacked in series and fitted with cooling fins. Both drifted with heat and age, and silicon replaced them.
Does a failing selenium rectifier give off hydrogen selenide?
The chapter rates the claim that failing selenium rectifiers give off hydrogen selenide as Untested. Popular sources name that gas, but the US toxicological profile says selenium dioxide forms when selenium is heated in air, and no emission measurement was found. NIOSH sets hydrogen selenide at 0.05 ppm with an IDLH of 1 ppm, and selenium compounds at 0.2 mg/m³ as Se.
How efficient were early battery-charging rectifiers?
The Bureau of Standards measured early battery-charging rectifiers in 1924. With 24 lead cells on charge, one aluminum electrolytic rectifier gave 55 to 59 percent, not counting transformer loss. The best tantalum cell result was near 42 percent, a vibrating-contact unit 43 percent, and gas-filled tube chargers with hot filaments 32 to 35 percent. For battery charging, check the code in force where you are.
Selected sources
- F. Braun, Ueber die Stromleitung durch Schwefelmetalle, Annalen der Physik und Chemie 153 (1874)
- J. C. Bose, Detector for Electrical Disturbances, US Patent 755,840 (1904)
- G. W. Pickard, US Patent 836,531 (1906)
- G. L. Pearson and W. H. Brattain, History of Semiconductor Research, Proceedings of the IRE 43 (1955)
- L. O. Grondahl, Unidirectional Current Carrying Device, US Patent 1,640,335 (1927)
- US Navy, NEETS Module 7, Introduction to Solid-State Devices and Power Supplies, NAVEDTRA 14179A (2012)
- H. D. Holler and J. P. Schrodt, Theory and Performance of Rectifiers, NBS Technologic Paper 265 (1924)
- J. A. Fleming, US Patent 803,684 (1905)
- L. de Forest, US Patents 841,387 (1907) and 879,532 (1908)
- J. Bardeen and W. H. Brattain, US Patent 2,524,035
- NIOSH Pocket Guide to Chemical Hazards, Hydrogen selenide and Selenium
- ATSDR, Toxicological Profile for Selenium
- How do copper-oxide and selenium rectifiers work?
- Glossary: Cat's-whisker detector
- Glossary: Crystal radio
Related chapters
This chapter is in Volume II: System Anatomies. Drafted and twice audited; chapter text final. Formats and prices · All chapters